Rare earth magnet and method for manufacturing the same

Number of patents in Portfolio can not be more than 2000

United States of America Patent

APP PUB NO 20020057982A1
SERIAL NO

09955306

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

Rare earth alloy powder having an oxygen content of 50 to 4000 wt. ppm and a nitrogen content of 150 to 1500 wt. ppm is compacted by dry pressing to produce a compact. The compact is impregnated with an oil agent and then sintered. The sintering process includes a first step of retaining the compact at a temperature of 700.degree. C. to less than 1000.degree. C. for a period of time of 10 to 420 minutes and a second step of permitting proceeding of sintering at a temperature of 1000.degree. C. to 1200.degree. C. The average crystal grain size of the rare earth magnet after the sintering is controlled to be 3 .mu.m to 9 .mu.m.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
NEOMAX CO LTD4-7-19 KITAHAMA CHUO-KU OSAKA-SHI OSAKA 541-0041

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Kuniyoshi, Futoshi Osaka, JP 51 237
Morimoto, Hitoshi Asago-gun, JP 39 367

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation