Production of active nickel powder and transformation thereof into nickel carbonyl

Number of patents in Portfolio can not be more than 2000

United States of America Patent

APP PUB NO 20070034053A1
SERIAL NO

10537069

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

Active nickel powder is produced by reducing a feed material, containing one or more reducible nickel salts, such that when nickel chloride is present, the weight ratio of chloride to total nickel is greater than 0.1 and the reducible nickel salts have a surface area in excess of 1 m.sup.2/g, with a reducing gas containing preferably at least 20 volume per cent hydrogen, at a temperature preferably between 300.degree. C. and 600.degree. C., and when nickel chloride is not present, by adding hydrogen chloride directly to the reducing gas. The resulting active nickel powder can be rapidly converted into nickel carbonyl by reaction with a gas containing carbon monoxide preferably at atmospheric or super-atmospheric pressure, in the absence of conventional carbonylation catalysts.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
FALCONBRIDGE LIMITEDTORONTO ONTARIO M5L 1B4

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Collins, Michael Sudbury, CA 119 2558
Kuula, Sandra Marie Cal Caron, CA 2 8

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation