ETHYLENE-PROPYLENE-DIENE RUBBER FOAMED MATERIAL AND SEALING MATERIAL

Number of patents in Portfolio can not be more than 2000

United States of America Patent

APP PUB NO 20140220334A1
SERIAL NO

14346173

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

An ethylene-propylene-diene rubber foamed material is obtained by foaming a rubber composition containing an ethylene-propylene-diene rubber. The ethylene-propylene-diene rubber foamed material has a permanent compression set obtained by being compressed by 50% at 80° C. for 22 hours to be then released at 23° C. after the elapse of 24 hours of 30% or less. The content ratio of a sulfur atom calculated based on the measurement result of a fluorescent X-ray measurement, based on mass, is 1000 ppm or less.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
NITTO DENKO CORPORATION1-2 SHIMOHOZUMI 1-CHOME IBARAKI-SHI OSAKA 567-8680

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Iwase, Takayuki Osaka, JP 43 107
Kawata, Joji Osaka, JP 6 9

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation