PROCESS FOR PRODUCING HIGH MOLECULAR WEIGHT POLYETHYLENE

Number of patents in Portfolio can not be more than 2000

United States of America Patent

APP PUB NO 20140329921A1
SERIAL NO

14361938

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

In a process for producing polyethylene, ethylene is contacted under polymerization conditions with a slurry of a catalyst composition comprising a particulate support and a Group 4 metal complex of a phenolate ether ligand carried by the support and present in an amount so as to provide about 0.1 to about 35 μιηo of Group 4 metal per gram of the support. The resultant polyethylene has a molecular weight of at least 3×105 g/mol as determined by ASTM 4020, an average particle size, d50, of less 300 microns, preferably about 100 to 250 microns, and a span, log10(d90/d10), of less than 0.4.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
TICONA GMBHAN DER B 43 65451 KELSTERBACH

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Hufen, Julia Rheinberg, DE 20 207
Robert, Dominique Dinslaken, DE 18 299

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation