METHOD OF MANUFACTURING COMPOSITE CRUCIBLE AND METHOD OF MANUFACTURING SILICON CRYSTAL

Number of patents in Portfolio can not be more than 2000

United States of America Patent

SERIAL NO

14818243

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A composite crucible 10 is characterized in the use of mullite (3Al2O3.2SiO2) as the basic material of the crucible. The composite crucible 10 has a crucible body 11 made of mullite material whose main component is alumina and silica, and a transparent vitreous silica layer 12 formed on the inner surface of the crucible body 11. The thickness of the transparent vitreous silica layer 12 is smaller than that of the crucible body 11. The crucible body 11 is formed by the slip casting method, and the transparent vitreous silica layer 12 is formed by the thermal spraying method.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
SUMCO CORPORATION1-2-1 SHIBAURA MINATO-KU TOKYO 105-8634

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
FUJITA, Takeshi Akita-shi, JP 268 3417
KANDA, Minoru Akita-shi, JP 42 552
KISHI, Hiroshi Akita-shi, JP 143 1432
KITAHARA, Ken Akita-shi, JP 29 92
SUDO, Toshiaki Akita-shi, JP 56 140
SUZUKI, Koichi Akita-shi, JP 389 3939
YOSHIOKA, Takuma Akita-shi, JP 14 30

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation