MOLYBDENUM DISULFIDE POWDER AND METHOD FOR MANUFACTURING THE SAME, METHOD FOR DEGRADING AN ORGANIC MATERIAL AND METHOD FOR STERILIZING

Number of patents in Portfolio can not be more than 2000

United States of America Patent

SERIAL NO

15163696

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A method for manufacturing a molybdenum disulfide powder includes conducting a precursor solution preparation step and a hydrothermal synthesis step. The precursor solution preparation step includes providing sodium molybdenum oxide dehydrate and thiourea, and conducting a mixing step. In the mixing step, an acid solution is mixed with the sodium molybdenum oxide dehydrate and the thiourea by titrating so as to form a precursor solution. In the hydrothermal synthesis step, the precursor solution is put into a hydrothermal container for reacting at a temperature ranging from 100° C. to 350° C. for 8 hours to 40 hours, thus the molybdenum disulfide powder is formed.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
NATIONAL TSING HUA UNIVERSITYHSINCHU CITY 30013

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
CHANG, Wei-En Miaoli County, TW 6 105
WU, Jyh-Ming Hsinchu County, TW 10 127

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation