Sheet adhesive and adhesion process using the same

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 10633512
APP PUB NO 20170349789A1
SERIAL NO

15603860

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

It has conventionally been difficult to achieve a sheet adhesive which adheres in a low temperature (from 20 to 90° C.), and has both of softness and high adhering strength. The present invention realizes a sheet adhesive capable of adhering in a low temperature (from 20 to 90° C.) which exhibits a high adhesiveness in spite of being a soft sheet of thin film, by forming a simulated multiple layer by using an elastomer as a substrate layer, and by forming a reactive layer by means of spraying or application.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
THREE BOND CO LTDTOKYO JAPAN TOKYO METROPOLIS

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Arai, Yoshihide Hachioji, JP 16 72
Kimura, Hiroshi Hachioji, JP 313 3789

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation

Maintenance Fees

Fee Large entity fee small entity fee micro entity fee due date
7.5 Year Payment $3600.00 $1800.00 $900.00 Oct 28, 2027
11.5 Year Payment $7400.00 $3700.00 $1850.00 Oct 28, 2031
Fee Large entity fee small entity fee micro entity fee
Surcharge - 7.5 year - Late payment within 6 months $160.00 $80.00 $40.00
Surcharge - 11.5 year - Late payment within 6 months $160.00 $80.00 $40.00
Surcharge after expiration - Late payment is unavoidable $700.00 $350.00 $175.00
Surcharge after expiration - Late payment is unintentional $1,640.00 $820.00 $410.00