Provided is a method for efficiently producing tungsten carbide from a raw material mixture comprising at least one valuable containing tungsten. The present invention relates to a method for producing tungsten carbide, comprising the steps of subjecting a raw material mixture comprising at least one valuable containing tungsten to electrolysis using an organic electrolytic solution to dissolve tungsten in the electrolytic solution; and calcining the electrolytic solution containing dissolved tungsten at a temperature of 800° C. or more to obtain tungsten carbide.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

  • JX NIPPON MINING & METALS CORPORATION

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Kawamura, Toshifumi Hitachi, JP 15 33

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation

Maintenance Fees

Fee Large entity fee small entity fee micro entity fee due date
7.5 Year Payment $3600.00 $1800.00 $900.00 Sep 12, 2026
11.5 Year Payment $7400.00 $3700.00 $1850.00 Sep 12, 2030
Fee Large entity fee small entity fee micro entity fee
Surcharge - 7.5 year - Late payment within 6 months $160.00 $80.00 $40.00
Surcharge - 11.5 year - Late payment within 6 months $160.00 $80.00 $40.00
Surcharge after expiration - Late payment is unavoidable $700.00 $350.00 $175.00
Surcharge after expiration - Late payment is unintentional $1,640.00 $820.00 $410.00