ALKOXYSILANE-MODIFIED POLYAMIC ACID SOLUTION, LAMINATE AND FLEXIBLE DEVICE EACH PRODUCED USING SAME, AND METHOD FOR PRODUCING LAMINATE

Number of patents in Portfolio can not be more than 2000

United States of America

SERIAL NO

16542471

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A (A) polyamic acid solution which can be (i) used to form a film that does not peel off even in a case where the film has a large thickness, and (ii) stably stored at a room temperature, and (B) a laminate that can be suitably used for production of a flexible device. An alkoxysilane-modified polyamic acid solution that can be obtained by reacting (a) an alkoxysilane compound containing the amino group and (b) a polyamic acid solution, and has a molar ratio of 0.980 or more and 0.9995 or less, which molar ratio is obtained by dividing a total number of moles of an aromatic tetracarboxylic dianhydride by a total number of moles of an aromatic diamine.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
KANEKA CORPORATION3-18 NAKANOSHIMA 2-CHOME KITA-KU OSAKA-SHI OSAKA 5308288 ?5308288

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Akinaga, Takahiro Otsu-shi, JP 4 8
Ozawa, Shinji Otsu-shi, JP 30 580
Takiguchi, Yuki Otsu-shi, JP 12 31

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation