A die-casting aluminum alloy without heat-treatment and a preparation method and application thereof. Based on a total weight of the die-casting aluminum alloy, the die-casting aluminum alloy includes: 6.0 to 8.0 wt % of Si; 0.3 to 1.2 wt % of Mg; 0.4 to 0.8 wt % of Cu; 0.1 to 0.3 wt % of Fe; 0.6 to 0.8 wt % of Mn; 0.05 to 0.20 wt % of Ti; 0.03 to 0.07 wt % of Sr; 0.03 to 0.07 wt % of Ce; 0.01 to 0.04 wt % of La; 0.01 to 0.1 wt % of Zr; less than or equal to 0.01 wt % of other impurity elements; and a balance of Al.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
XIAOMI EV TECHNOLOGY CO LTDBEIJING 100176

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
BAI, Yongchang Beijing, CN 1 0
WU, Xinxing Beijing, CN 5 6
YANG, Dong Beijing, CN 180 1586

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation