Corrosion resistant austenitic stainless steel containing 0.1 to 0.3 percent manganese

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 4222773
SERIAL NO

06043240

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

An austenitic stainless steel which is completely or practically completely austenitic in a hot worked, solution treated state, with properties characteristic for such steel and with a corrosion resistance clearly superior to the AISI 304 type of 18/8-steel, at least on a par with AISI 316 type of acid resistant steel 17/12-2Mo. The steel consists essentially of less than 0.10% C, less than 1.5% Si, between 0.10 and 0.30% Mn, between 17 and 20% Cr, between 6 and 16% Ni, between 2.0 and 4.0% Cu, less than 0.40% N, less than 1.0% Ti, less than 1.5% Nb and less than 100 ppm B, the balance being iron and impurities such as S, P and Mo usually present in steel.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

  • FAGERSTA AB

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Degerbeck, Jorgen Fagersta, SE 1 5

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation