Process for the recovery of zinc, copper and cadmium in the leaching of zinc calcine

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 4383979
SERIAL NO

06181651

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

Zinc, copper and cadmium are recovered from their ferrites by subjecting the ferrites to a sulfuric acid bearing solution in the presence of potassium, sodium or ammonium ions under atmospheric conditions at 80.degree.-105.degree. C. to precipitate the iron present in the ferrites as jarosite, separating at least a portion of the jarosite-bearing solid material from the solution before recycling the solution to a neutral leach, from which a copper and cadmium bearing solution is recovered and to which acid and calcine are also fed, feeding the solid obtained from the neutral leach to the said ferrite treatment stage classifying the solid obtained from the neutral leach into a finer and coarser fraction, feeding the finer fraction to the ferrite treatment stage, comminuting the coarser fraction by grinding, leaching or milling and recycling the comminuted fraction to the process.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
OUTOKUMPU OYTOOLONKATU 4 HELSINKI

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Bjorkqvist, Lars-Goran Kokkola, FI 2 7
Gisler, Raija-Leena Altdorf, CH 1 5
Liukkonen, Simo S Espoo, FI 1 5
Rastas, Jussi K Pori, FI 11 49

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation