Recovery of cobalt and nickel from sulphidic material

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 4594102
SERIAL NO

06532331

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A process for recovering cobalt and nickel values from cobalt and nickel containing sulphidic material also containing iron includes roasting the sulphidic material to produce a calcine containing water soluble cobalt and nickel sulphate, and leaching the calcine in aqueous sulphate solution under oxidizing conditions at an oxygen overpressure in the range of from about 50 kPa to about 1500 kPa and at a temperature in the range of from about 100.degree. to about 180.degree. C. to produce an iron-containing residue and a cobalt and nickel containing solution. The residue is separated from the solution, and cobalt and nickel values are recovered from the solution.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
698638 ALBERTA LTDBOX 3388 FORT SASKATCHEWAN ALBERTA T8L 2

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Chalkley, Michael E St. Albert, CA 6 42
Kerfoot, Derek E Fort Saskatchewan, CA 2 12
Weir, Donald R Fort Saskatchewan, CA 26 398

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation