Process for preparing powder of an alloy of a rare earth element, iron and boron for a resin bonded magnet

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 4944801
SERIAL NO

07375459

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A powder of a rare earth oxide, or a powder of a rare earth oxide and a rare earth metal is mixed with a powder containing iron, a powder containing boron and at least one material selected from among an alkali metal, an alkaline earth metal and a hydrogenated product thereof. The mixture is heated at a temperature of 900.degree. C. to 1200.degree. C. in a non-oxidizing atmosphere, subjected to wet treatment, and heated again at a temperature of 650.degree. C. to 1100.degree. C., whereby an alloy powder is obtained. Alternatively, the mixture is heated at a temperature of 900.degree. C. to 1200.degree. C., crushed into coarse particles, heated again at a temperature of 650.degree. C. to 1100.degree. C. and subjected to wet treatment. The powder is pulverized into a finer powder having an average particle diameter of 1 to 10 microns. The powder is used for making a magnet with a resin.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
SUMITOMO METAL MINING CO LTD 11-3 5-CHOME SHINBASHI MINATO-KU TOKYO JAPANNot Provided

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Ishikawa, Takashi Ichikawa, JP 176 1685
Ohmori, Kenji Ichikawa, JP 40 337
Oshimura, Nobumitsu Ichikawa, JP 1 2

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation