A process for producing a Cu-Fe-Co-Ti alloy useful as conductor elements in the electronics and connector industries. The alloy is produced in the form of a bath having a Ti/Fe+Co ratio between 0.3 and 1 and a Co/Fe ratio between 0.10 and 0.90. The molten alloy bath is deoxidized with boron, cast, homogenized, cold drawn, and subjected to a precipitation heat treatment at a temperature lower, by at most 80.degree. C., than a temperature TM leading to the maximum electric conductivity.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
TREFIMETAUX S AF-92411 COURBEVOIE

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Gandossi, Christian Seifontaine, FR 1 3
Mineau, Laurent Grenoble, FR 1 3
Picault, Alain Mantes-la-Ville, FR 1 3

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation