Nickel (or other transition metal) contaminated with about 5 ppm technetium is decontaminated by dissolving the nickel and the technetium into an aqueous acid solution while introducing a graphite or activated carbon powder into the acid to immediately adsorb the dissolving technetium. The technetium-contaminated powder is separated from the aqueous acid solution and the nickel is then electrowon from the solution. The depleted acid solution is then recycled back to the dissolution step.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
DURATEK SERVICES INC10100 OLD COLUMBIA ROAD COLUMBIA MD

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Ayers, Laura J Knoxville, TN 4 49
Boris, Gregory F Knoxville, TN 7 78
Gass, William R Plum Boro, PA 4 67
Snyder, Thomas S Oakmont, PA 39 345

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation