Method of densifying crosslinked fibers

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 5252275
SERIAL NO

07665761

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A method is disclosed for the densification of crosslinked fibers having a crosslinking agent loading level of from about 2.5 molar to about 5 molar %. The crosslinked fibers are compressed from an initial density of from about 0.02 g/cc to about 0.04 g/cc to a second density of from about 0.20 g/cc to about 1.00 g/cc by either the simultaneous or sequential application of heat and pressure. The surface temperature of the press is typically between about 60.degree. C. to about 180.degree. C. The compression force for the air laid or wet laid webs is in the range of about 800 psi to about 115,000 psi. Densifying the crosslinked fiber in this manner produces a compressed web having enhanced absorbent capacities of from about 21 g/g to about 15 g/g.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
WEYERHAEUSER NR COMPANYPO BOX 9777 CH1J27 FEDERAL WAY WA 98063-9777

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Graef, Peter A Tacoma, WA 40 2732
Howard, Fred B Gig Harbor, WA 22 1775
Sultze, Rolland F Everett, WA 2 80

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation