Production of fiber pulp by impregnating the lignocellulosic material with an aqueous alcoholic SO.sub.2 solution prior to defibration

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 5338405
SERIAL NO

07842365

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

In a process for manufacturing chemo-mechanical and/or chemothermal-mechanical wood pulps, raw materials containing lignocellulose, such as wood shavings, wood chips, pre-ground wood or sawdust, are first impregnated with an aqueous alcoholic SO.sub.2 solution and then heated to a temperature between 50.degree. and 170.degree. C. for a period of 1 to 300 minutes. The wood shavings are then ground to the desired degree of fineness in a defibrinating device. The process makes it possible to achieve up to 50% reduction in grinding energy in comparison with known chemothermal-mechanical processes.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
STORA FELDMUBLE AKTIENGESELLSCHAFTFELDMUHLEPLATZ 1 D-4000 DUSSELDORF 11

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Patt, Rudolf Reinbek, DE 9 120
Rachor, Georg Grossostheim, DE 1 23

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation