Process for the electrodeposition of an amorphous cobalt-iron-phosphorus alloy

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 5435903
SERIAL NO

07974668

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A thin amorphous alloy of cobalt, iron and phosphorus having good workability and the ability to be used as a soft magnetic material is formed by electrolytic deposition. The electrolytic bath has a pH of 1.0 to 2.2 and contains at least a divalent cobalt ion, a divalent iron ion, and phosphorous acid and/or a phosphite. The amorphous alloy contains at least 69 atomic percent cobalt, 2 to 30 atomic percent phosphorus and the iron/(cobalt+iron) atomic ratio is from 0.001 to 0.1. The alloy may be deposited on a working electrode having a chrome-plated surface with a center line average roughness of less than 1 .mu.m and may be peeled from the electrode to obtain a tape-shaped or foil-shaped product.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

  • MITSUBISHI RAYON CO., LTD.

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Kamada, Kensuke Hiroshima, JP 15 276
Oda, Masaharu Hiroshima, JP 10 246
Ohashi, Hidehiko Hiroshima, JP 10 153

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation