Ni/metal hydride accumulator

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 5500309
SERIAL NO

08346897

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

The positive electrode of a Ni/metal hydride accumulator is formed from a mass mixture of Ni(OH).sub.2 and an oxidation-resistant graphite. The stable graphite is notable for a high degree of crystallinity and a low ash content. In conventional Ni/metal hydride accumulators, cobalt compounds play an essential part in developing a conductive matrix within their positive nickel hydroxide electrodes, leading to reductive destruction of the matrix by severe high temperature short circuit testing. In contrast, the same accumulators, with positive electrodes produced according to the present invention, survive the test with only a temporary and slight decline in capacity.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
NBT GMBHAM LEINEUFER 51 D-30419 HANNOVER

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Hofmann, Gunter Hofheim, DE 17 594
Kleinsorgen, Klaus Kelkheim, DE 6 73
Lichtenberg, Frank Zeiskam, DE 5 57

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation