Abstract

See full text

Microcrystalline bodies based on .alpha.-Al.sub.2 O.sub.3 are made by drying sub-micron powders, press compacting and shock sintering at an intermediate sinter temperature range of 1,300.degree. to 1,550.degree. C., i.e. bringing the compact up to such range in under 60 seconds, preferably under 10.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
KORUND LAUFENBURG GMBHFERROWEG 1 D-79725 LAUFENBURG

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Moltgen, Paul Laufenburg, DE 5 85
Schmoll, Josef Goslar, DE 13 193
Wilhelm, Pirmin Bad Sackingen, DE 3 147

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation