Process for production of chemically prestressed glass

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 5846280
SERIAL NO

08842431

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

The process for producing a chemically prestressed glass of very high surface quality includes subjecting an Li.sub.2 O-free starting glass from the SiO.sub.2 -Al.sub.2 O.sub.3 -M.sub.2 O-MO system which also contains TiO.sub.2, CeO.sub.2 and F.sub.2 to chemical ion exchange by immersing it in a potassium salt bath at a temperature between 350.degree. C. and 550.degree. C. and at a residence time of between 0.5 and 20 hours to form the chemically prestressed glass. In a preferred embodiment of the process, the potassium salt bath contains a potassium nitrate melt and the glass is polished after prestressing. The chemically prestressed glass is particularly useful for making hard disks.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
SCHOTT AGHATTENBERGSTRASSE 10 55122 MAINZ

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Speit, Burkhard Mainz, DE 31 464

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation