A hardenable white gold alloy consists essentially of about 55-60 % gold, about 12-20% silver, about 8-15% copper, about 8-18% palladium, about 0.0-1.0% tin, zinc indium or cobalt, and, optionally, about 0.005-0.02% iridium and/or ruthenium, and also about 0.01-0.03 weight percent lithium. The alloy is nickel-free, but has a pleasing white color similar to that of nickel-containing white gold alloys. The alloy has a fine grain structure, a lower hardness in its annealed condition, but is capable of being hardened to an exceptional hardness value. The hardening procedure is reversible.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
HALLMARK SWEET INC49 PEARL STREET ATTLEBORO MA 02703

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Agarwal, Dwarika P Attleboro, MA 16 116
Raykhtsaum, Grigory Norton, MA 18 55

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation