A hard film is covered on the outer circumferential surface of a piston ring by means of an arc ion plating. The hard film has a mixture of crystal structure of CrN and crystal structure of Mo.sub.2 N containing oxygen in a solid solution state, and comprises chromium at 40 to 78 percent by weight, molybdenum at 3 to 35 percent by weight, oxygen at 3 to 20 percent by weight and the remainder of nitrogen. The crystal particle size is less than 1 .mu.m. The Vickers hardness is within a range from 1600 to 2500. The film thickness is preferably 1 to 60 .mu.m. Carbon in a solid solution state at 0.5 to 8 percent by weight may be substituted for the oxygen. Alternatively, both oxygen and carbon may be contained in a solid solution state with oxygen at 3 to 20 percent by weight, carbon at 0.5 to 8 percent by weight with the total content of carbon and oxygen within 25 percent by weight.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
TEIKOKU PISTON RING CO LTDNISHIDA TAKASHI PILLS THE CAPITAL OF TOKYO JAPAN NO 6 NO 2 DINGMU

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Ito, Naoki Okaya, JP 284 2331
Tanaka, Shoji Shiojiri, JP 160 2045
Yamashita, Nobuyuki Shiojiri, JP 138 2921

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation