Method for making Fe-based soft magnetic alloy

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 6083325
SERIAL NO

08893768

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A method for making a Fe-based soft magnetic alloy where an alloy melt is injected onto a moving cooling unit to form an amorphous alloy ribbon. The alloy melt contains Fe as a main component, B and at least one metallic element M selected from the group consisting of Ti, Zr, Hf, V, Nb, Ta, Mo and W, the composition of the alloy melt being selected such that the resulting amorphous alloy ribbon is characterized by a first crystallization temperature at which fine grain bcc Fe crystallites precipitate, and a second crystallization temperature at which a compound phase containing Fe--B and/or Fe--M precipitates. The amorphous alloy ribbon is then annealed at a temperature which is higher that the first crystallization temperature and less than the second crystallization temperature for an annealing time in the range of 0 minutes to 20 minutes.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
ALPS ELECTRIC CO LTDJAPAN
JAPAN SCIENCE AND TECHNOLOGY CORPORATION1-8 HONCHO 4-CHOME KAWAGUCHI-SHI SAITAMA 332-0012
AKIHISA INOUE11-806 KAWAUCHIJUTAKU 35BANCHI MOTOHASEKURA AOBA-KU SENDAI MIYAGI
TSUYOSHI MASUMOTO3-8-22 KAMISUGI AOBA-KU SENDAI MIYAGI

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Bitoh, Teruo Niigata-ken, JP 4 33
Hatanai, Takashi Niigata-ken, JP 42 416
Hayakawa, Yasuo Niigata-ken, JP 31 480
Inoue, Akihisa Miyagi-ken, JP 197 2954
Makino, Akihiro Niigata-ken, JP 85 867
Masumoto, Tsuyoshi Miyagi-ken, JP 105 1726

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation