In a process for producing welded steel pipes, a pipe is molded cold from a TM-rolled sheet, welded together and sized to the desired diameter, whereby the sheet includes steel with (in wt. %) 0.02 to 0.20% carbon, 0.05 to 0.50% silicon, 0.50 to 2.50% manganese, 0.003 to 0.06% aluminum, the remainder being iron with potentially other production-related impurities. After welding and sizing, the pipe is subjected to a heat treatment process at a temperature of 100-300.degree. C. and for a holding time that is suited to the thickness of the pipe wall, with subsequent cooling with air or by forced cooling. The resulting pipe is resistant to aging and has sufficiently integral deformation reserve against fracturing with the same high degree of strength, without exceeding the upper limit for the ratio of yield strength to tensile stress according to the current industry standards for conventional steels.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
MANNESMANNROHREN-WERKE AG45473 MÜLHEIM A D RUHR

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Hohl, Gerold Neuss, DE 2 15
Knauf, Gerhard Duisburg, DE 3 17

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation