See full text

When a pitch composition prepared by mixing 100 parts by weight of mesophase pitch with 10 to 1,000 parts by weight of coal tar pitch, is heat-treated at a temperature of 500° C. or higher, it is possible to produce a high-density coke at a high yield while avoiding the foaming of the mesophase pitch. In addition, when the coke is graphitized at a temperature of 2,000° C. or higher, it is possible to obtain an artificial graphite having a high graphitization degree. Further, when the coke is first pulverized and then graphitized at a temperature of 2,000° C. or higher, it is possible to obtain a high-crystallinity graphite powder which can be suitably used as a carbon material for a negative electrode of non-aqueous solvent type secondary battery having a high discharge capacity and a high charge-discharge efficiency.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
MITSUBISHI GAS CHEMICAL COMPANY INC5-2 MARUNOUCHI 2-CHOME CHIYODA-KU TOKYO 1008324

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Fujiura, Ryuji Ibaraki, JP 8 63
Kanno, Koichi Ibaraki, JP 11 50
Tsuruya, Hirotaka Ibaraki, JP 16 53

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation