Alloying fine adjustment method

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 7591875
APP PUB NO 20080121072A1
SERIAL NO

11943911

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

The present invention discloses a type of alloying fine adjustment method in which alloy materials are pulverized into micropowder and fed via the conventional powder spraying system; the said alloy materials are fed into the upper part of the spraying tank of the spraying system whose spraying pipelines are connected to the aerated bricks at the bottom of the molten steel container. Based on the existing argon blowing and mixing system, argon is taken as the carrier and used to pressurize the alloy powders into the aerated bricks at the bottom of the molten steel container via the spraying system and further into the molten steel container for the sake of alloying fine adjustment. After the alloy powders are fed, continue blowing and mixing argons until the alloy powders and the molten steels are evenly mixed in the molten steel container to complete the alloying process. This method features such advantages as short alloying time, good alloying effects, high yield of alloys and absence of pollution.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
HUATIAN ENGINEERING & TECHNOLOGY CORPORATION MMCNO 25 HUNAN ROAD MAANSHAN 243005

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Zhou, Jianan Maanshan , CN 2 0

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation