A Ni—Pt alloy and target superior in workability containing 0.1 to 20 wt % Pt and having a Vickers hardness of 40 to 90. A method of manufacturing the Ni—Pt alloy comprises steps of subjecting a raw material Ni having a purity of 3N level to electrochemical dissolution, neutralizing the electrolytically leached solution with ammonia, removing impurities through filtration with activated carbon, blowing carbon dioxide into the resultant solution to form nickel carbonate, exposing the resultant product to a reducing atmosphere to prepare high purity Ni powder, leaching a raw material Pt having a purity of 3N level with acid, subjecting the leached solution to electrolysis to prepare high purity electrodeposited Pt, and dissolving the resultant high purity Ni powder and high purity electrodeposited Pt. The method enables rolling of the Ni—Pt alloy ingot upon reducing the hardness thereof, which results in the stable and efficient manufacture of a rolled target.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
JX NIPPON MINING & METALS CORPORATION6-3 OTEMACHI 2-CHOME CHIYODA-KU TOKYO 1008164

International Classification(s)

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Shindo, Yuichiro Ibaraki, JP 59 650

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation