Method of producing a friction texturized polyester filament yarn and yarn made thereby

Number of patents in Portfolio can not be more than 2000

United States of America Patent

PATENT NO 5579629
SERIAL NO

08047794

Stats

ATTORNEY / AGENT: (SPONSORED)

Importance

Loading Importance Indicators... loading....

Abstract

See full text

The friction texturized polyester filament yarn has a titer of 400 to 600 dtex and a crimpability of at least 45% and can be provided with at least 60 slubs/m. The method of making this friction texturized polyester filament yarn comprises texturizing a flat yarn with a titer of 400 to 600 dtex at a rate of at least 350 m/min and a yarn tension ratio, F2/F1, less than one via a squeezing twister. A set yarn can be made from the friction texturized polyester yarn with the titer of 400 to 600 dtex by heating.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

  • RHONE-POULENC VISCOSUISSE SA

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address # of filed Patents Total Citations
Fischer, Klaus Lucetne, CH 179 3029

Cited Art Landscape

Load Citation

Patent Citation Ranking

Forward Cite Landscape

Load Citation