PROCESS FOR PRODUCING IMPROVED GRAIN REFINING ALUMINIUM-TITANIUM-BORON MASTER ALLOYS FOR ALUMINUM FOUNDRY ALLOYS

World Intellectual Property Organization Patent

APP PUB NO WO-2010097658-A1
SERIAL NO

PCTIB2009050808

Stats

Importance

Loading Importance Indicators... loading....

Abstract

See full text

A process is provided for producing aluminium-titanium-boron grain refining master alloys containing soluble titanium aluminide and insoluble aluminium boride particles, the process comprising mixing aluminium-boron alloy powder and K2TiF6 salt to obtain a blended mixture, heat treating the mixed powder blend thus obtained in an inert gas furnace just below the melting point of aluminium, at approximately 650 degrees Celcius sufficiently long and compacting the heated powder blend in the form of tablets. The cast grain size of an aluminium-7 wt% silicon foundry alloy after inoculation with this master alloy at an addition level of 0.02% Ti was less than 200 microns for contact times of upto 15 minutes.

Loading the Abstract Image... loading....

First Claim

See full text

Family

Loading Family data... loading....

Patent Owner(s)

Patent OwnerAddress
TUBITAKTR06100 ANKARA

International Classification(s)

  • [Classification Symbol]
  • [Patents Count]

Inventor(s)

Inventor Name Address
BIROL YUCEL 41470 KOCAELI

Cited Art Landscape

Load Citation